Discussion Stainless Steel Etchants for Foundry Applications
#9
There are definitely alternatives out there, but they may well not be as effective or versatile as the nitric/hydrochloric acid mixture. Any individuals use citric acid or ferric chloride, but they may not provide you the same level of depth in your delineate.